A286 superalloy


Your Search returned these results: page: « 1 »

A-286 High Strength Iron-Based Superalloy – Properties, Composition, Heat Treatments and Specificati
A-286 is an age-hardenable iron base superalloy for applications requiring high strength from -320°F up to 1000°F long time, 1300-1500°F short time. Oxidation resistance is high for continuous service to 1500°F, intermittent to 1800°F. Detailed properties are supplied along with applications.

page: « 1 »


University of Surrey-Short Courses and MSc in Materials science
CILAS state of the art laser particle size analyzers
Materials Science books by Elsevier
X-Ray diffractometers from Shimadzu

 

version 2.0 - AZoM™ - The A to Z of Materials and AZojomo - The "AZo Journal of Materials Online"...AZoM™.com Pty.Ltd Copyright © 2000-2009