  • Article - 10 Sep 2012
    Stainless steels are known as high-alloy steels. They contain about 4-30% of chromium. They are further divided into martensitic, austenitic, and ferritic steels. Another group of stainless steels are...
  • Article - 6 Sep 2012
    Alloy steels comprise a wide variety of steels with compositions that exceed the limitations of Si, Va, Cr, Ni, Mo, Mn, B and C allocated for carbon steels. In comparison with carbon steels, alloy...
  • Article - 30 Aug 2012
    Aluminum alloys are sensitive to high temperatures. They tend to lose some of their strength when exposed to high temperatures of about 200-250°C.
  • Article - 30 Aug 2012
    Aluminum alloys are good low-temperature alloys as they gain strength when exposed to subzero temperatures. They have strong corrosion resistance characteristics and high electrical conductivity.
  • Article - 16 Aug 2012
    This data page covers the C61800 copper alloy which displays have high corrosion resistance. Other properties such as mechanical, thermal and fabrications are described along with chemical...
  • Article - 10 Aug 2012
    Brass is an alloy mainly consisting of copper and zinc. Brass alloys can be easily shaped and are available in various colors. Brass has high thermal conductivity. UNS C37700 forging brass alloys have...
  • Article - 2 Aug 2012
    UNS C17510 beryllium copper alloys are available in mill hardened tempers and heat treatable and ductile tempers. These alloys have moderate strength and about 50% IACS conductivity.
  • Article - 2 Aug 2012
    UNS C17500 copper-cobalt-beryllium alloys comprise moderate strength and about 50% IACS conductivity. These alloys are available in mill hardened tempers and heat treatable and ductile tempers.
  • Article - 1 Aug 2012
    Pure copper has high electrical and thermal conductivity. Alloys can be freely formed by the copper. The UNS 11300 silver-bearing tough Pitch copper has 101% IACS conductivity, and high ductility. It...
  • Article - 2 Jul 2012
    Hot rolled AISI 1022 steel is a low hardenability carbon steel with low tensile strength ranging between 360-560 MPa.