Search

Search Results
Results 3181 - 3190 of 3278 for Mechanical components
  • Article - 30 Aug 2012
    Aluminum alloys are good low-temperature alloys as they gain strength when exposed to subzero temperatures. They have strong corrosion resistance characteristics and high electrical conductivity.
  • Article - 22 Aug 2012
    The UNS C97800 alloy is a leaded nickel bronze copper alloy. Other types of bronze alloys include phosphor bronze, tin bronze, aluminum bronze, silicon bronze, architectural bronze and manganese...
  • Article - 18 Aug 2012
    Copper-nickel alloys have very good resistance to biofouling and marine corrosion, and possess good fabricability. Copper gains more strength and corrosion resistance when nickel is added to it.
  • Article - 16 Aug 2012
    Aluminium bronze is an alloy, which consist of about 6% of nickel and iron, and 9 to 12% of aluminium. It has a golden color. UNS C62500 copper alloys have good corrosion resistance. They are...
  • Article - 16 Aug 2012
    This data page covers the C61800 copper alloy which displays have high corrosion resistance. Other properties such as mechanical, thermal and fabrications are described along with chemical...
  • Article - 10 Aug 2012
    UNS C34000 medium leaded brass is alloy of copper, zinc and lead. It has good corrosion resistance and formability. It is produced by the processes such as blanking, heading, upsetting, machining,...
  • Article - 10 Aug 2012
    Brass is an alloy mainly consisting of copper and zinc. Brass alloys can be easily shaped and are available in various colors. Brass has high thermal conductivity. UNS C37700 forging brass alloys have...
  • Article - 7 Aug 2012
    Pure copper has good electrical and thermal conductivity. More than 400 varieties of copper alloys are available. UNS C18150 chromium copper alloys have high strength and wear resistance at elevated...
  • Article - 2 Aug 2012
    UNS C17510 beryllium copper alloys are available in mill hardened tempers and heat treatable and ductile tempers. These alloys have moderate strength and about 50% IACS conductivity.
  • Article - 2 Aug 2012
    UNS C17500 copper-cobalt-beryllium alloys comprise moderate strength and about 50% IACS conductivity. These alloys are available in mill hardened tempers and heat treatable and ductile tempers.