Aluminum Bronze Forging (UNS C63200) - Mechanical Properties

Aluminum bronze UNS C63200 has a copper content of not less than 82%.

The following table shows the mechanical properties of UNS C63200 forging as a function of heat treatment and thickness.

Temper Thickness Tensile Str. Yield Str. Elong. Rockwell
B C F 30T
O50 127 mm. (5in.) 689MPa (100ksi) 310MPa (45ksi) 22% 92 - - -

Equivalent materials to UNS C63200 copper alloy are provided in the table below.

  • ASTM B124
  • ASTM B150
  • ASTM B283

The chemical composition of UNS C63200 copper alloy is outlined in the following table.

Element Content (%)
Aluminum, Al 8.7-9.5
Nickel, Ni 4.0-4.8
Iron, Fe 3.5-4.3
Manganese, Mn 1.2-2.0
Silicon, Si 0.1
Lead, Pb 0.02
Copper, Cu Remainder

Tell Us What You Think

Do you have a review, update or anything you would like to add to this article?

Leave your feedback
Your comment type
Submit

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.