Dec 3 2012
Semi-red brass UNS C84000 has a copper content of not less than 82%.
The following table shows the mechanical properties of UNS C84000 casting alloy as a function of heat treatment.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
M01 |
214MPa (31ksi) |
110MPa (16ksi) |
15% |
|
255MPa (37ksi) |
117MPa (17ksi) |
24% |
The chemical composition of UNS C84000 copper alloy is outlined in the following table.
Element |
Content (%) |
Copper, Cu |
82-89 |
Zinc, Zn |
5-14 |
Tin, Sn |
2-4 |
Nickel, Ni |
0.5-2 |
Iron, Fe |
0.4 |
Boron, B |
0.2 |
Zirconium, Zr |
0.2 |
Sulfur, S |
0.1-0.65 |
Lead, Pb |
0.09 |
Phosphorous, P |
0.05 |
Antimony, Sb |
0.02 |
Silicon, Si |
0.005 |
Aluminum, Al |
0.005 |