Jan 16 2013
Leaded yellow brass UNS C85700 has a copper content of not less than 58%.
Tabulated below are the mechanical properties of UNS C85700 centrifugal cast alloy as a function of heat treatment.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
M02 |
276MPa (40ksi) |
97MPa (14ksi) |
15% |
The chemical composition of UNS C85700 copper alloy is outlined in the following table.
Elements |
Content (%) |
Copper, Cu |
58.0-64.0 |
Zinc, Zn |
32.0-40.0 |
Nickel, Ni |
1.0 |
Tin, Sn |
0.50-1.5 |
Lead, Pb |
0.8-1.5 |
Aluminum, Al |
0.8 |
Iron, Fe |
0.7 |
Silicon, Si |
0.05 |
Equivalent materials to UNS C85700 copper alloy are given in the table below.
- ASTM B176
- ASTM B271
- ASTM B30
- ASTM B584
- ASTM B763
- QQ C390