UNS C87610 copper alloy has a copper content of not less than 90%.
The following table shows the mechanical properties of UNS C87610 centrifugal cast alloy as a function of heat treatment.
| Temper |
Tensile Str. |
Yield Str. |
Elong. |
| M02 |
310 MPa (45 ksi) |
124 MPa (18 ksi) |
20% |
The chemical composition of UNS C87610 copper alloy is outlined in the following table.
| Element |
Content (%) |
| Copper, Cu |
90 |
| Silicon, Si |
3-5 |
| Zinc, Zn |
3-5 |
| Manganese, Mn |
0.25 |
| Iron, Fe |
0.2 |
| Lead, Pb |
0.09 |
Equivalent materials to UNS C87610 copper alloy include:
- ASTM B30
- ASTM B584
- ASTM B763