Dec 12 2012
Leaded tin bronze UNS C92700 has a copper content of not less than 86%.
The following table shows the mechanical properties of UNS C92700 continuous cast alloy as a function of heat treatment.
| Temper |
Tensile Str. |
Yield Str. |
Elong. |
| M07 |
262MPa (38ksi) |
138MPa (20ksi) |
8% |
Equivalent materials to UNS C92700 copper alloy are provided below:
- ASTM B30
- ASTM B505
- QQ C390
- SAE J461
- SAE J462
The chemical composition of UNS C92700 copper alloy is outlined in the following table.
| Element |
Content (%) |
| Copper, Cu |
86-89 |
| Tin, Sn |
9-11 |
| Lead, Pb |
1.0-2.5 |
| Nickel, Ni |
1 |
| Zinc, Zn |
0.7 |
| Phosphorus, P |
0.25 |
| Antimony, Sb |
0.25 |
| Iron, Fe |
0.2 |
| Sulfur, S |
0.05 |
| Aluminum, Al |
0.005 |
| Silicon, Si |
0.005 |