Gold Nanorods (Axial Diameter - 10 nm)

Strem Chemical's Gold Nanorods, with axial diameter 10 nm (±10%), all have a Peak Axial Surface Plasmon Resonance Wavelength of 512 nm. They should be stored at approximately 4°C for up to 6 months and should not be frozen.

The physical and chemical properties of Gold Nanorods are outlined in the following:

Properties

Wavelength 808 nm

Wavelength 780 nm Wavelength 750 nm Wavelength 700 nm

Color and Form

pale red liquid

pale red solution pale red liquid pale red-brown liquid

Concentration

36 ug/ml (±10%)

35 ug/ml (±10%) 34 ug/ml (±10%) 30 ug/ml (±10%)

Longitudinal Size (nm)

41 (±10%)

38 (±10%) 35 (±10%) 29 (±10%)

Catalog Number

79-6035

79-6030 79-6025 79-6020

Strem Chemicals also supply Gold Nanorods with an axial diameter of 25 nm.

This information has been sourced, reviewed and adapted from materials provided by Strem Chemicals.

For more information on this source, please visit Strem Chemicals.

Citations

Please use one of the following formats to cite this article in your essay, paper or report:

  • APA

    Strem Chemicals. (2019, January 29). Gold Nanorods (Axial Diameter - 10 nm). AZoM. Retrieved on May 21, 2019 from https://www.azom.com/article.aspx?ArticleID=4675.

  • MLA

    Strem Chemicals. "Gold Nanorods (Axial Diameter - 10 nm)". AZoM. 21 May 2019. <https://www.azom.com/article.aspx?ArticleID=4675>.

  • Chicago

    Strem Chemicals. "Gold Nanorods (Axial Diameter - 10 nm)". AZoM. https://www.azom.com/article.aspx?ArticleID=4675. (accessed May 21, 2019).

  • Harvard

    Strem Chemicals. 2019. Gold Nanorods (Axial Diameter - 10 nm). AZoM, viewed 21 May 2019, https://www.azom.com/article.aspx?ArticleID=4675.

Ask A Question

Do you have a question you'd like to ask regarding this article?

Leave your feedback
Submit