UNS C18200 chromium copper alloy has a copper content of no less than 99.1%.
The following table outlines the mechanical properties of UNS C18200 plates as a function of heat treatment and thickness.
Temper |
Thickness |
Tensile Str. |
Yield Str. |
Elong. |
Rockwell |
B |
C |
F |
30T |
TF00 |
51 mm (2 in) |
400 MPa (58 ksi) |
290 MPa (42 ksi) |
25% |
70 |
- |
- |
- |
|
76 mm (3 in) |
386 MPa (56 ksi) |
276 MPa (42 ksi) |
25% |
70 |
- |
- |
- |