Fire-Refined Tough Pitch Copper Rods UNS C12900 - Mechanical Properties

Fire-refined tough pitch copper UNS C12900 has a copper content of not less than 99.88%.

The following table shows the mechanical properties of UNS C12900 rods as a function of heat treatment and thickness.

Temper Thickness Tensile Str. Yield Str. Elong. Rockwell Shear Str.
B C F 30T
M20 25.4mm (1in) 221MPa (32ksi) 69MPa (10ksi) 55% - - 40 - 152MPa (22ksi)
OS050 25.4mm (1in) 221MPa (32ksi) 69MPa (10ksi) 55% - - 40 - 152MPa (22ksi)

Equivalent materials to UNS C12900 copper alloy are the following:

  • ASTM B224
  • MIL B-20292

Tell Us What You Think

Do you have a review, update or anything you would like to add to this article?

Leave your feedback
Your comment type
Submit

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.