Sep 27 2012
UNS C50580 copper alloy has a copper content of not less than 98.5%.
The following table shows the mechanical properties of UNS C50580 flat products as a function of heat treatment.
| Temper |
Tensile Str. |
Elong. |
| H01 |
400 MPa (58 ksi) |
24% |
| H02 |
448 MPa (65 ksi) |
12% |
| H04 |
510 MPa (74 ksi) |
8% |
| H06 |
552 MPa (80 ksi) |
6% |
| H08 |
586 MPa (85 ksi) |
3% |
| OS015 |
365 MPa (53 ksi) |
50% |
The chemical composition of UNS C50580 copper alloy is outlined in the following table.
| Element |
Content (%) |
| Tin, Sn |
1.0-1.7 |
| Zinc, Zn |
0.3 |
| Lead, Pb |
0.05 |
| Fe |
0.05-0.20 |
| Nickel, Ni |
0.05-0.20 |
| Phosphorous, P |
0.01-0.35 |
| Copper, Cu |
Balance |