Dec 10 2012
The following table shows the mechanical properties of UNS C82510 sand cast alloy as a function of heat treatment.
|
Temper |
Tensile Str. |
Elong. |
Rockwell |
|
B |
C |
F |
30T |
|
TB00 |
552MPa (80ksi) |
10% |
- |
- |
- |
- |
|
TF00 |
1104MPa (160ksi) |
1% |
- |
- |
- |
- |
The chemical composition of UNS C82510 copper alloy is outlined in the following table.
|
Element |
Content (%) |
|
Beryllium, Be |
1.9-2.15 |
|
Cobalt, Co |
1-1.2 |
|
Iron, Fe |
0.25 |
|
Silicon, Si |
0.2-0.35 |
|
Nickel, Ni |
0.2 |
|
Aluminum, Al |
0.15 |
|
Tin, Sn |
0.1 |
|
Zinc, Zn |
0.1 |
|
Chromium, Cr |
0.09 |
|
Lead, Pb |
0.02 |
|
Copper, Cu |
Remainder |