Nov 14 2012
UNS C95700 has a copper content of not less than 71%.
Tabulated below are the mechanical properties of UNS C95700 continuous cast alloy as a function of heat treatment.
| Temper | Tensile Str. | Yield Str. | Elong. | 
| M07 | 610MPa (90ksi) | 275MPa (40ksi) | 15% | 
The chemical composition of UNS C95700 copper alloy is outlined in the following table.
| Elements | Content (%) | 
| Copper, Cu | 71 | 
| Manganese, Mn | 11.0-14.0 | 
| Aluminum, Al | 7.0-8.5 | 
| Iron, Fe | 2.0-4.0 | 
| Nickel, Ni | 1.5-3.0 | 
| Silicon, Si | 0.1 | 
Equivalent materials to UNS C95700 copper alloy are:
- ASTM B148 
- ASTM B30 
- ASTM B505 
- QQ C390